In-vivo degradation of middle-term highly cross-linked and remelted polyethylene cups: Modification induced by creep, wear and oxidation

http://hdl.handle.net/10076/00016975
http://hdl.handle.net/10076/00016975
12aaad1a-cece-47ee-a41e-95d10fc5a8f9
名前 / ファイル ライセンス アクション
2015DM032.pdf 2015DM032 (6.2 MB)
Item type 学位論文 / Thesis or Dissertation(1)
公開日 2017-07-04
タイトル
タイトル In-vivo degradation of middle-term highly cross-linked and remelted polyethylene cups: Modification induced by creep, wear and oxidation
言語 en
言語
言語 eng
キーワード
主題Scheme Other
主題 UHMWPE
キーワード
主題Scheme Other
主題 Total hip arthroplasty
キーワード
主題Scheme Other
主題 Retrievals
キーワード
主題Scheme Other
主題 Raman spectroscopy
キーワード
主題Scheme Other
主題 FT-IR
キーワード
主題Scheme Other
主題 Oxidation
キーワード
主題Scheme Other
主題 Wear
キーワード
主題Scheme Other
主題 Creep
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_db06
資源タイプ doctoral thesis
アクセス権
アクセス権 open access
アクセス権URI http://purl.org/coar/access_right/c_abf2
著者 三浦, 良浩

× 三浦, 良浩

en Miura, Yoshihiro

ja-Kana ミウラ, ヨシヒロ

ja 三浦, 良浩

Search repository
抄録
内容記述タイプ Abstract
内容記述 In this study Raman (RS) and Fourier Transform In frared (FT-IR) spectroscopic techniques were exploited to study 11 retrieved liners made of remelted highly cross-linked polyethylene (HXLPE), with the intent to elucidate their in-vivo mechanical and chemical degradation.The retrievals had different follow-ups, ranging from af ew months to 7 years of implantation time and belong to the first generation of highly cross-linked and remelted polyethylene clinically introduced in 1999, but still currently implanted. Raman assessments enabled to discriminate contributes of wear and creep on the total reduction of thickness in different locations of the cup. According to our results, although the most of the viscoelastic deformation occurred during the first year (bedding-in period), it progressed during the steady wear state up to 7 years with much lower but not negligible rate. Overall, the wear rate of this remelt HXLPE liner was low. Preliminary analysis on microtomed sections of the liners after in-vivo and in-vitro accelerated aging (ASTM F2003-02) enabled to obtain a phenomenological correlation between the oxidation index (01) and the amount of orthorhombic phase fraction (αc), which can be easily non-destructively measured by RS. Profiles of αc,obtained from different locations of the cups were used to judge the oxidative degradation of the 11 retrievals, considering also the ex-vivo time elapsed from the revision surgery to the spectroscopic experiments. Low but measurable level of oxidation was detected in all the short-term retrievals, while in the middle-term samples peaks of 01 were observed in the subsurface (up to 01=4.5), presumably induced by the combined effect of mechanical stress, lipid absorption and prolonged ex-vivo shelf-aging in air.
内容記述
内容記述タイプ Other
内容記述 本文 / Department of Orthopaedic Surgery, Mie University, Graduate School of Medicine
内容記述
内容記述タイプ Other
内容記述 12p
書誌情報
発行日 2016-03-25
DOI
識別子タイプ DOI
関連識別子 10.1016/j.jmbbm.2015.06.028
権利
権利情報 (C) 2015 Elsevier Ltd.
フォーマット
内容記述タイプ Other
内容記述 application/pdf
著者版フラグ
出版タイプ VoR
出版タイプResource http://purl.org/coar/version/c_970fb48d4fbd8a85
出版者
出版者 三重大学
出版者(ヨミ)
値 ミエダイガク
関係URI
関連名称 https://doi.org/10.1016/j.jmbbm.2015.06.028
学位名
学位名 博士(医学)
学位授与機関
学位授与機関識別子Scheme kakenhi
学位授与機関識別子 14101
学位授与機関名 三重大学
学位授与年月日
学位授与年月日 2016-03-25
学位授与番号
学位授与番号 甲医学第1769号
ノート
資源タイプ(三重大)
値 Doctoral Dissertation / 博士論文
戻る
0
views
See details
Views

Versions

Ver.1 2023-06-19 16:46:16.880298
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3